DOI

Original languageEnglish
Pages (from-to)1158-1167
JournalAdvanced engineering materials
Volume17
Issue number8
DOIs
StatusPublished - 2015

    Treatment code (Nähere Zuordnung)

  • Basic - Fundamental (Grundlagenforschung)

    Fields of Expertise

  • Advanced Materials Science

ID: 1752827